In IML (In-Mold Labeling) production, the dimensional accuracy of the label directly determines positioning accuracy during injection molding and the final product's appearance quality. A frequently overlooked but extremely critical factor is tension control.
Improper tension control causes the label to be unidirectionally stretched during printing, slitting, and die-cutting processes, resulting in dimensional changes – labels become longer, wider, or skewed. These tiny dimensional deviations may be only a few tenths of a millimeter on a single label, but when accumulated across an entire roll and then magnified through injection molding, they can lead to labels that cannot be precisely positioned in the mold, pattern shifts, exposed edges, or even entire batch scrappage.
This article provides a systematic explanation of how to solve label stretching and lengthening issues through static tension winding and unwinding control processes in IML label production, covering three dimensions: the principles of tension control, tension settings for each process step, and common problem troubleshooting.

The substrate of IML labels is plastic film (primarily PP or PE), not paper. Plastic film has elasticity – it stretches and deforms under stress, and this deformation does not fully recover after the stress is removed.
The typical IML label production process is: printing → slitting → die-cutting → injection molding. Throughout this process, the label film undergoes multiple cycles of winding, unwinding, pulling, and cutting. If tension control is inadequate at any step, the film will be unidirectionally stretched, causing label dimensions to change.
Chain reaction of dimensional deviation:
IML label die-cutting position deviation should not exceed ±0.5mm, and die-cutting dimensional tolerances are subject to clear industry standards. Achieving this precision requires stable, controllable tension throughout the entire process from printing to die-cutting.
IML label substrate is film material. During printing, slitting, die-cutting, and other processes, tension mainly comes from the following sources:
Unwinding tension: Resistance from the unwinding shaft as the roll material is pulled out. Excessive tension stretches the film before it even enters the printing unit.
Pulling tension: The pulling force exerted by pull rollers between various process steps. Speed differences between pull points cause tension fluctuations.
Rewinding tension: Tension during finished product winding. Excessive rewinding tension deforms the label material, affecting subsequent die-cutting accuracy.
Printing unit tension: Tension generated by speed differences between color groups during printing, directly affecting registration accuracy.
Difference from pressure-sensitive labels: Compared to pressure-sensitive labels, the unwinding and rewinding tension during in-mold label printing should be considerably lower. This is because IML labels lack a backing paper support, and the film itself has limited tensile strength.
Excessive unwinding tension deforms the in-mold label material, causing registration errors in subsequent printing; excessive rewinding tension deforms the in-mold label material, causing inaccuracies in subsequent die-cutting.
Unwinding tension is the first checkpoint in tension control.
The direct consequence of excessive unwinding tension: the film is already stretched before entering the printing unit. When the stretched film enters printing, the pattern will lengthen, and this stretching is irreversible – even after printing is complete, the film will not "shrink back."
Control points:
During printing, the film needs to run smoothly between color groups. If tension fluctuates, registration accuracy cannot be guaranteed.
Control points:
Slitting is the process of cutting large rolls into narrower rolls that meet requirements. Tension control during slitting directly affects the width consistency of the finished labels.
Control points:
Die-cutting is the final dimensional shaping step in IML label production. Tension control during die-cutting directly determines the label's final shape and dimensions.
Die-cutting equipment needs to complete die-cutting, counting, stacking, and waste winding under tension control.
Control points:
| Tension Issue | Direct Manifestation | Subsequent Impact |
|---|---|---|
| Excessive unwinding tension | Film stretched and lengthened | Registration errors, pattern distortion |
| Excessive rewinding tension | Label rolls overwound | Dimensional deviation during die-cutting, increased scrap rate |
| Excessive machine direction tension | Label curls inward | Label cannot lie flat against mold during injection |
| Inconsistent tension across processes | Dimensional batch variation | Positioning errors when loaded into machine |
| Tension fluctuations | Registration deviation, die-cutting offset | Inconsistent batch dimensions |
The following parameters are industry reference values. Actual production settings should be adjusted based on film material, thickness, width, and other factors:
| Process Step | Recommended Tension Range | Control Method | Notes |
|---|---|---|---|
| Unwinding | Minimum that does not stretch film | Automatic tension controller | Automatically reduces tension as roll diameter decreases |
| Printing | Uniform and stable, consistent across color groups | Closed-loop tension control | Multi-stage independent control |
| Slitting | Slightly lower than printing tension | Independent tension control | Different widths set separately |
| Die-cutting | Consistent with printing tension | Constant tension control | Waste winding controlled separately |